File:Wood-salts-damage-efflorescence-PUR-met-AIC-News.jpg
From MediaWiki

Size of this preview: 473 × 600 pixels. Other resolution: 2,288 × 2,902 pixels.
Original file (2,288 × 2,902 pixels, file size: 2.44 MB, MIME type: image/jpeg)
Wood. Efflorescence formed after storage with open-cell polyester polyurethane.
Comments: Dendritic, white amine deposits formed on the wood object, after it was wrapped in polyethylene sheeting and placed on polyethylene foam for approximately 5 years.
Image credit: Photograph by Adriana Rizzo, © The Metropolitan Museum of Art. AIC, permission received 6/10/2020 from B. Naugle via email to rarenstein.
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 15:31, 7 August 2020 | ![]() | 2,288 × 2,902 (2.44 MB) | Eguerard (talk | contribs) | Wood. Efflorescence formed after storage with open-cell polyester polyurethane. Comments: Dendritic, white amine deposits formed on the wood object, after it was wrapped in polyethylene sheeting and placed on polyethylene foam for approximately 5 yea... |
You cannot overwrite this file.
File usage
The following page uses this file: