File:Formate-efflorescence-crystal on glass.png
From MediaWiki

Size of this preview: 800 × 525 pixels. Other resolution: 937 × 615 pixels.
Original file (937 × 615 pixels, file size: 507 KB, MIME type: image/png)
Summary[edit | edit source]
Glass. Crystals caused by offgassing storage materials. Comments: Pollutants from off-gassing storage materials caused acetate salts to form on black glass beads. Image credit: Photograph by Dr. Katherine Curran. Permission received 9/1/2020 from Katherine Curran via email to DThickett and SSpringer.
File history
Click on a date/time to view the file as it appeared at that time.
Date/Time | Thumbnail | Dimensions | User | Comment | |
---|---|---|---|---|---|
current | 20:26, 26 March 2021 | ![]() | 937 × 615 (507 KB) | Sspringer (talk | contribs) | Glass. Crystals caused by offgassing storage materials. Comments: Pollutants from off-gassing storage materials caused acetate salts to form on black glass beads. Image credit: Photograph by Dr. Katherine Curran. Permission received 9/1/2020 from Katherine Curran via email to DThickett and SSpringer. |